Standard: GB /T 14 - 1988
Available sizes: M10 to M8 (4 sizes)
| Standard Body | Standard Number |
|---|---|
| GB | GB /T 14 |
| NF | NF E 27-351 |
| DIN | DIN 603 |
| ISO | ISO 8677 |
| UNI | UNI 5732 |
| ANSI | ANSI/ASME B 18.5.2.3M |
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal |
|---|
| ds_nominal |
|---|
| M10 | 2.00 | 15.76 | 16.43 | 34 | 10.45 | 38 | 44 | 8.90 | 7.55 | 36.60 | 9.55 |
| M12 | 3.00 | 23.72 | 24.52 | 50.8 | 17.55 | 54 | 60 | 13.10 | 11.45 | 53.90 | 16.45 |
| M6 | 1.25 | 7.8 | 8.36 | 17.3 | 5.40 | 22 | 28 | 4.48 | 3.6 | 19.10 | 4.60 |
| M8 | 1.75 | 11.76 | 12.43 | 27.16 | 8.45 | 30 | 36 | 6.48 | 5.6 | 29.30 | 7.55 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
© 2026 Ningbo Ruixi Metal Surface Technology Co., Ltd.. All rights reserved.