Standard: UNI 6104 - 1975
Available sizes: (M14) to M12 (3 sizes)
| Size | P | k_max | k_min | s_max | s_min | ds_max | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|
| (M14) | 2.5 | 40.8 | 39.2 | 22 | 50 | 22 | 40 | 20 |
| M10 | 1.75 | 24.65 | 23.35 | 12 | 30 | 12 | 24 | 12 |
| M12 | 2 | 32.8 | 31.2 | 16 |
| 38 |
| 16 |
| 32 |
| 16 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.