Standard: KS B 1002
Available sizes: M10 to M8 (6 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| M10 | 3 | 10.3 | 14.78 | 26.4 | 33.6 | 9 | 0.2 | 15 | 15.22 | 0.8 | 39.98 |
| M3 | 0.7 | 1.9 | 2.68 | 4.7 | 5.9 | 2.1 | 0.15 |
| 2.8 |
| 2.92 |
| 0.4 |
| 7.66 |
| M4 | 1 | 2.63 | 3.85 | 6.8 | 8.9 | 3 | 0.15 | 4 | 4.15 | 0.5 | 11.05 |
| M5 | 1.5 | 4.28 | 6.22 | 11.2 | 14.6 | 4.5 | 0.15 | 6.4 | 6.58 | 0.6 | 17.77 |
| M6 | 2 | 5.96 | 8.62 | 15.7 | 19.6 | 6 | 0.15 | 8.8 | 8.98 | 0.6 | 23.35 |
| M8 | 2.5 | 8.5 | 12.28 | 22.4 | 28.2 | 7.5 | 0.2 | 12.5 | 12.72 | 0.8 | 33.53 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.