Standard: GB /T 32076.8 - 2017
Available sizes: (M22) to M20 (4 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| (M22) | 4 | 2 | 21.95 | 67 | 58.5 | 42.4 | 37 | 23 | 24.05 | 35 | 30 |
| M12 | 2 | 1.2 | 9.25 | 30 | 27.9 | 18.83 | 16.43 |
| 10 |
| 10.75 |
| 15.57 |
| 13 |
| M16 | 2.5 | 1.2 | 13.1 | 41 | 38.5 | 26.4 | 22.52 | 14 | 14.9 | 21.48 | 18 |
| M20 | 3 | 2 | 16.1 | 50 | 42.8 | 32.84 | 27.84 | 17 | 17.9 | 26.16 | 22 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.