Standard: DIN 580 - 2024
Available sizes: M10 to M8 (7 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| M10 | 35.0 | 11.5 | 12 | 62.5 | 64.1 | 34.5 | 36.1 | 33.9 | 35.5 | 63.0 | 35.0 |
| M12 | 40.0 | 13.5 | 14 | 71.5 | 73.1 | 39.5 | 41.1 | 38.9 | 40.5 | 72.0 | 40.0 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
| M14 | 50.0 | 17.5 | 18 | 89.4 | 91.2 | 49.4 | 51.2 | 48.8 | 50.6 | 90.0 | 50.0 |
| M16 | 65.0 | 21.4 | 22 | 107.3 | 109.5 | 64.3 | 66.3 | 58.7 | 60.7 | 108.0 | 60.0 |
| M18 | 75.0 | 25.3 | 26 | 125.2 | 127.7 | 74.3 | 76.5 | 68.5 | 70.7 | 126.0 | 70.0 |
| M6 | 20.0 | 5.5 | 6 | 35.5 | 37.1 | 19.5 | 20.9 | 19.1 | 20.5 | 36.0 | 20.0 |
| M8 | 30.0 | 9.5 | 10 | 53.5 | 55.1 | 29.5 | 30.9 | 29.1 | 30.5 | 54.0 | 30.0 |
© 2026 Ningbo Ruixi Metal Surface Technology Co., Ltd.. All rights reserved.