Standard: ASME B 18.2
Available sizes: M10 to M8 (4 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| M10 | 2.50 | 46 | 18.90 | 29.16 | 34.64 | 20.00 | 19.67 | 43.00 | 3.00 | 30.00 | 32.66 |
| M5 | 1.00 | 18 | 6.60 | 9.64 | 11.55 | 6.00 | 5.82 |
| 14.20 |
| 1.10 |
| 10.00 |
| 10.80 |
| M6 | 1.50 | 26 | 10.40 | 14.57 | 17.32 | 10.00 | 9.78 | 22.30 | 1.50 | 15.00 | 16.32 |
| M8 | 2.00 | 34 | 13.70 | 20.16 | 24.25 | 14.00 | 13.73 | 30.50 | 2.10 | 21.00 | 22.58 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.