Standard: DIN 6334
Available sizes: M10 to M8 (7 sizes)
| Size | P | k_max | s_max | s_min | k_nominal |
|---|---|---|---|---|---|
| M10 | 2 | 122 | 24 | 48 | 26.75 |
| M12 | 2.5 | 240 | 30 | 60 | 33.53 |
| M14 | 3 | 412 | 36 | 72 | 39.98 |
| M16 | 3.5 | 825 | 46 | 90 | 50.85 |
| M18 | 4 | 1470 | 55 | 108 | 60.79 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
| M6 | 1.25 | 18 | 13 | 24 | 14.38 |
| M8 | 1.75 | 63 | 19 | 36 | 21.1 |