Standard: DIN 935
Available sizes: M12 to M24 (4 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| M12 | 2 | 24 | 4.98 | 26.17 | 19 | 16 | 17.3 | 13.5 | 4.5 | 21.7 | 16.9 |
| M16 | 3 | 36 | 5.98 | 39.55 | 27 | 24 | 25.9 |
| 19.9 |
| 5.5 |
| 33.2 |
| 24.9 |
| M20 | 3.5 | 46 | 7.58 | 50.85 | 33 | 30 | 32.4 | 24.4 | 7 | 42.7 | 30.5 |
| M24 | 3.5 | 50 | 7.58 | 55.37 | 35 | 33 | 35.6 | 26 | 7 | 46.6 | 32.5 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.