Standard: GB 6176 - 1986
Available sizes: M10 to M8 (5 sizes)
| Standard Body | Standard Number |
|---|---|
| GB | GB /T 6176 |
| DIN | DIN EN ISO 8674 |
| ISO | ISO 8674 |
| UNI | UNI 5587 |
| Size | P | e | r | k_max | k_min | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|
| M10 | 1.5 | 9.4 |
| 10.7 |
| 14 |
| 19. |
| 0.60 |
| 14.1 |
| 13.4 |
| 15.1 |
| 23.35 |
| M12 | 2 | 13.3 | 15.2 | 20.00 | 27.70 | 0.80 | 20.3 | 19 | 21.60 | 32.95 |
| M14 | 2 | 19.1 | 21.8 | 30.00 | 42.7 | 0.80 | 28.6 | 27.3 | 32.40 | 50.85 |
| M16 | 3 | 23.2 | 26.5 | 36.00 | 51.1 | 0.80 | 34.7 | 33.1 | 38.90 | 60.79 |
| M8 | 1 | 6.3 | 7.1 | 10.00 | 14.6 | 0.60 | 9.3 | 8.94 | 10.80 | 17.77 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.