Standard: CNS 9674 - 1988
Available sizes: (M2.2) to M3 (6 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| (M2.2) | 0.45 | 0.1 | 0.95 | 1.65 | 1.35 | 5.3 | 4.9 | 2.5 | 1.32 | 1.5 | 1 |
| (M2.3) | 0.5 | 0.1 | 1.01 | 2.05 | 1.75 | 6.3 | 5.8 |
| 3.6 |
| 1.53 |
| 1.9 |
| 2 |
| (M2.6) | 0.8 | 0.2 | 2.29 | 3.3 | 2.9 | 10.3 | 9.7 | 4.9 | 2.83 | 3.1 | 2 |
| M2 | 0.45 | 0.1 | 0.75 | 1.45 | 1.15 | 4.7 | 4.3 | 2.3 | 1.11 | 1.3 | 1 |
| M2.5 | 0.7 | 0.2 | 1.6 | 2.7 | 2.3 | 8.3 | 7.8 | 4.2 | 2.13 | 2.5 | 2 |
| M3 | 1.25 | 0.4 | 3.78 | 5.1 | 4.5 | 16.4 | 15.6 | 7.7 | 4.36 | 4.8 | 3 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.