Standard: ASME B 18.6
Available sizes: 0# to 2# (6 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 0# | 0.1120 | 0.169 | 0.030 | 0.069 | 0.059 | 40 | 0.257 | 0.031 | 0.040 | 0.241 | 0.039 |
| 00# | 0.0860 | 0.129 | 0.022 | 0.053 | 0.044 | 56 | 0.194 |
| 0.023 |
| 0.031 |
| 0.180 |
| 0.031 |
| 000# | 0.0600 | 0.087 | 0.014 | 0.037 | 0.029 | 80 | 0.131 | 0.016 | 0.022 | 0.119 | 0.023 |
| 0000# | 0.0340 | 0.051 | 0.009 | 0.022 | 0.018 | 120 | 0.077 | 0.009 | 0.013 | 0.071 | 0.013 |
| 1# | 0.1380 | 0.211 | 0.037 | 0.086 | 0.074 | 32 | 0.321 | 0.039 | 0.050 | 0.303 | 0.048 |
| 2# | 0.1640 | 0.254 | 0.045 | 0.102 | 0.088 | 32 | 0.384 | 0.045 | 0.058 | 0.364 | 0.054 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
© 2026 Ningbo Ruixi Metal Surface Technology Co., Ltd.. All rights reserved.