Standard: DIN 7504
Available sizes: ST2.9 to ST4.2 (3 sizes)
| Standard Body | Standard Number |
|---|---|
| GB | GB /T 15856.2 |
| DIN | DIN EN ISO 15482 |
| ISO | ISO 15482 |
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| ST2.9 | 1.3 | 0.7~2.25 | 2.8 |
| 2.35 |
| 1.4 |
| 1.3 |
| 7.3 |
| 4.4 |
| 4.3 |
| 6.9 |
| 2 |
| ST3.5 | 1.6 | 1.75~4.4 | 4.1 | 2.8 | 2.0 | 1.6 | 9.3 | 5.2 | 5.1 | 8.9 | 2 |
| ST4.2 | 1.8 | 2~6 | 5.8 | 3.15 | 2.4 | 1.8 | 11.3 | 6.8 | 6.8 | 10.9 | 3 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.