Standard: GB /T 15856.5 - 2023
Available sizes: ST2.9 to ST4.2 (3 sizes)
| Standard Body | Standard Number |
|---|---|
| GB | GB /T 15856.5 |
| DIN | DIN EN ISO 15480 |
| ISO | ISO 15480 |
| UNI | UNI 8117 |
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| ST2.9 |
| 1.3 |
| 0.25 |
| 0.1 |
| 7.6 |
| 5.96 |
| 1.3 |
| 0.6 |
| 3 |
| 1.5 |
| 8.3 |
| 3.4 |
| ST3.5 | 1.6 | 0.3 | 0.2 | 9.8 | 8.71 | 1.6 | 0.9 | 3.8 | 2.2 | 10.5 | 4.3 |
| ST4.2 | 1.8 | 0.5 | 0.25 | 12.2 | 10.95 | 1.8 | 1 | 5.3 | 3.1 | 13.5 | 5.9 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.