Standard: ASME B 18.6
Available sizes: 0# to 6# (7 sizes)
| Size | P | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|
| 0# | 0.0730 | 0.038 | 0.026 | 0.142 | 0.130 | 0.027 | 0.018 | 0.046 | 0.019 |
| 1# | 0.0990 | 0.051 | 0.035 | 0.193 | 0.180 | 0.036 | 0.026 | 0.060 | 0.027 |
| 2# |
| 0.1250 |
| 0.065 |
| 0.043 |
| 0.245 |
| 0.231 |
| 0.045 |
| 0.034 |
| 0.075 |
| 0.035 |
| 3# | 0.1510 | 0.079 | 0.048 | 0.296 | 0.281 | 0.054 | 0.041 | 0.089 | 0.039 |
| 4# | 0.1900 | 0.099 | 0.060 | 0.373 | 0.357 | 0.068 | 0.053 | 0.110 | 0.050 |
| 5# | 0.2500 | 0.130 | 0.075 | 0.492 | 0.473 | 0.087 | 0.070 | 0.144 | 0.064 |
| 6# | 0.3125 | 0.162 | 0.084 | 0.615 | 0.594 | 0.106 | 0.085 | 0.178 | 0.072 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.