Standard: ASME B 18.6
Available sizes: 2# to 7# (6 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 2# | 0.0990 | 0.095 | 0.061 | 0.038 | 0.028 | 28 | 0 | 0.145 | 0.070 | 0.070 | 0.161 |
| 3# | 0.1250 | 0.120 | 0.078 | 0.065 | 0.050 | 20 | 1R |
| 0.187 |
| 0.088 |
| 0.091 |
| 0.205 |
| 4# | 0.1510 | 0.144 | 0.094 | 0.065 | 0.050 | 19 | 1R | 0.229 | 0.105 | 0.091 | 0.248 |
| 5# | 0.1900 | 0.180 | 0.118 | 0.075 | 0.060 | 16 | 2R | 0.292 | 0.130 | 0.112 | 0.313 |
| 6# | 0.2500 | 0.237 | 0.155 | 0.095 | 0.080 | 14 | 3R | 0.389 | 0.170 | 0.133 | 0.414 |
| 7# | 0.3750 | 0.355 | 0.233 | 0.100 | 0.085 | 12 | 4R | 0.590 | 0.253 | 0.191 | 0.622 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.