Standard: ASME B 18.6
Available sizes: 2# to 8# (6 sizes)
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 2# | 0.0990 | 0.035 | 0.055 | 0.067 | 0.102 | 0.187 | 0.169 | 0.018 | 1 | 0.078 | 0.052 |
| 3# | 0.1250 | 0.035 | 0.063 | 0.083 | 0.148 | 0.236 | 0.217 |
| 0.027 |
| 2 |
| 0.095 |
| 0.060 |
| 4# | 0.1640 | 0.064 | 0.090 | 0.107 | 0.172 | 0.309 | 0.287 | 0.030 | 2 | 0.120 | 0.088 |
| 5# | 0.2160 | 0.082 | 0.108 | 0.139 | 0.242 | 0.408 | 0.382 | 0.032 | 3 | 0.153 | 0.112 |
| 6# | 0.3125 | 0.144 | 0.170 | 0.198 | 0.302 | 0.590 | 0.557 | 0.040 | 3 | 0.216 | 0.174 |
| 8# | 0.3750 | 0.182 | 0.208 | 0.237 | 0.380 | 0.708 | 0.670 | 0.064 | 4 | 0.256 | 0.215 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.