Standard: GB /T 70.2 - 2015
Available sizes: M3 to M6 (4 sizes)
| Standard Body | Standard Number |
|---|---|
| GB | GB /T 70.2 |
| DIN | DIN EN ISO 7380(-1) |
| ISO | ISO 7380(-1) |
| ANSI | ASME/ANSI B 18.3.4M |
| Size | P | e | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|---|
| M3 |
| 0.7 |
| 1.95 |
| 2.20 |
| 3.8 |
| 4 |
| 4.7 |
| 7.60 |
| 6.84 |
| 2.873 |
| 7.24 |
| 3.82 |
| M4 | 1 | 3.0 | 3.3 | 6.0 | 6 | 6.8 | 10.50 | 9.57 | 4.583 | 10.07 | 5.82 |
| M5 | 1.5 | 5.2 | 5.5 | 10.0 | 10 | 11.2 | 17.50 | 16.57 | 6.863 | 17.07 | 9.78 |
| M6 | 2 | 8.44 | 8.80 | 16.0 | 16 | 17.7 | 28.00 | 26.68 | 11.429 | 27.48 | 15.73 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.