Standard: QC /T 890 - 2011
Available sizes: 01 to 02 (2 sizes)
| Size | P | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|
| 01 | NST5 | 1.2 | 2.4~2.6 | 3.1~3.7 | 10 | 12.5 | 19.2 | 11.8~12 | 9.35~9.5 |
| 02 | NST7 | 1.2 | 2.4~2.6 | 4.9~5.6 | 10 | 12.5 | 19.2 | 11.8~12 | 9.35~9.5 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.