Standard: UNI 5911 - 1966
Available sizes: M3 to M6 (4 sizes)
| Size | P | k_max | s_max | s_min | ds_max | ds_min | k_nominal |
|---|---|---|---|---|---|---|---|
| M3 | 0.7 | 14 | M4 | 4 | 6 | 6.75 | 3.88 |
| M4 | 1 | 18 | M6 | 6 | 9 | 9.9 | 5.88 |
| M5 | 1/1.25 | 22 | M8 | 8 | 12 | 13.1 | 7.85 |
| M6 |
| 1.25/1.75 |
| 30 |
| M12 |
| 12 |
| 18 |
| 19.1 |
| 11.82 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.