Standard: GB /T 32076.11 - 2024
Available sizes: M12 to M22 (4 sizes)
| Size | P | r | k_max | k_min | s_max | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|
| M12 | 16.75 | 17.85 | 3.7 | 4.3 | 16.85 | 29.48 | 0.8 | 25 | 30 | 6 |
| M16 | 23.05 | 24.15 | 3.7 | 4.3 | 23.15 | 38.38 | 0.8 | 33 | 39 |
| 7 |
| M20 | 28.3 | 29.4 | 4.4 | 5.6 | 28.4 | 49 | 0.8 | 43 | 50 | 7 |
| M22 | 37.75 | 38.85 | 5.4 | 6.6 | 37.85 | 64.8 | 0.8 | 56 | 66 | 7.5 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.