Standard: ANSI B 18.22
Available sizes: - to 8# (6 sizes)
| Size | P | e | r | k_max | k_min | s_min | ds_max | ds_min | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|---|---|
| - | 0.190 | 0.036 | 0.065 | 0.214 | 0.500 | 0.219 | 0.495 | 0.049 | 0.227 | 0.515 |
| 10# | 0.312 | 0.064 | 0.104 | 0.370 | 0.875 | 0.375 | 0.868 | 0.083 | 0.390 |
| 0.905 |
| 12# | 0.438 | 0.051 | 0.080 | 0.464 | 0.922 | 0.469 | 0.915 | 0.065 | 0.484 | 0.937 |
| 3/16 | 0.375 | 0.064 | 0.104 | 0.433 | 1.000 | 0.438 | 0.993 | 0.083 | 0.453 | 1.030 |
| 6# | 0.216 | 0.051 | 0.080 | 0.245 | 0.562 | 0.250 | 0.557 | 0.065 | 0.265 | 0.577 |
| 8# | 0.250 | 0.051 | 0.080 | 0.307 | 0.734* | 0.312 | 0.727 | 0.065 | 0.327 | 0.749 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
© 2026 Ningbo Ruixi Metal Surface Technology Co., Ltd.. All rights reserved.