Standard: DIN 6798
Available sizes: 1.7 to 3.7 (5 sizes)
| Standard Body | Standard Number |
|---|---|
| DIN | DIN 6798(A) |
| UNI | UNI 8842-A |
| Size | P | k_max | k_min | s_max | s_min | ds_max | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|
| 1.7 | 2.2 | 0.3 | 9 | 2.34 | 4.5 | M2 | 4.2 | 0.03 |
| 2.2 |
| 3.2 |
| 0.4 |
| 9 |
| 3.38 |
| 6 |
| M3 |
| 5.7 |
| 0.06 |
| 2.7 | 4.3 | 0.5 | 11 | 4.48 | 8 | M4 | 7.64 | 0.14 |
| 3.2 | 6.4 | 0.7 | 12 | 6.62 | 11 | M6 | 10.57 | 0.36 |
| 3.7 | 8.4 | 0.8 | 14 | 8.62 | 15 | M8 | 14.57 | 0.8 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.