Standard: ANSI B 18.8
Available sizes: Φ0.8 to Φ2 (5 sizes)
| Standard Body | Standard Number |
|---|---|
| EN | EN 28750 |
| GB | GB /T 879.4 |
| DIN | DIN EN ISO 8750 |
| ISO | ISO 8750 |
| ANSI | ANSI/ASME B 18.8.3M(S) |
| Size | P | k_max | k_min | s_max | s_min | ds_max | k_nominal | ds_nominal |
|---|---|---|---|---|---|---|---|---|
| Φ0.8 | 1.15 | 1.04 |
| 1 |
| 1.05 |
| 0.95 |
| 0.45 |
| 0.3 |
| 0.6 |
| Φ1 | 1.73 | 1.6 | 1.5 | 1.62 | 1.4 | 1.05 | 0.5 | 1.45 |
| Φ1.2 | 2.78 | 2.6 | 2.5 | 2.65 | 2.4 | 2.9 | 0.7 | 3.9 |
| Φ1.5 | 3.84 | 3.62 | 3.5 | 3.67 | 3.4 | 5.7 | 1 | 7.5 |
| Φ2 | 4.4 | 4.12 | 4 | 4.2 | 3.9 | 7.6 | 1.1 | 9.6 |
Standard corrosion protection for indoor and mild outdoor environments.
Salt spray: 96–200 hours | RoHS compliant (trivalent chromium)
High-performance coating for automotive, marine, and harsh environments.
Salt spray: 720–1500 hours | Recommended for grade 8.8+
Heavy-duty protection for structural and outdoor applications.
Salt spray: 500–1000 hours | Thread tolerance adjustment required
Note for high-strength fasteners (Grade 10.9, 12.9): Electroplating processes require hydrogen embrittlement relief baking (minimum 4 hours at 200°C within 4 hours of plating). Contact our engineering team for grade-specific plating recommendations.
Request detailed technical specifications, material certifications, and availability information for your application requirements. Our engineering team can provide product recommendations, custom specifications, and technical documentation.
© 2026 Ningbo Ruixi Metal Surface Technology Co., Ltd.. All rights reserved.